Pitting corrosion is a localized form of corrosion in passivated materials. The surface remains largely intact, while deep, often pinprick-like holes form in specific spots. This phenomenon is dangerous because the overall material loss remains minimal, but the component can be locally penetrated.
Mechanism
Stainless steel owes its durability to a passive layer of chromium oxide, only a few nanometers thick. Chloride ions can locally breach this layer at defects. At the fracture point, a small active anode is formed, surrounded by a large passive cathode. This unfavorable surface area ratio drives corrosion deeper into the steel.
Inside the hole, the pH level drops, chlorides accumulate, and the process sustains itself (autocatalysis). From the outside, often only a small dot is visible.
Favorable factors
- Chloride in water, salt solutions, cleaning agents or seawater atmosphere
- Elevated temperature – the critical pitting temperature (CPT) is material-specific
- Temper colors and scale after welding: chromium-depleted zones under the oxide layer
- Cracks, deposits, coatings – an oxygen-depleted environment develops beneath them
- Rough or contaminated surfaces, especially foreign rust caused by iron particles
PREN – Total Effectiveness
Resistance to pitting corrosion is estimated via the effective sum PREN ( Pitting Resistance Equivalent Number ):
PREN = %Cr + 3,3 × %Mo + 16 × %N
Higher values indicate higher durability. 1.4301 achieves approximately 18, while 1.4404, due to its molybdenum content, achieves approximately 24 to 26. Duplex and superaustenitic alloys are significantly higher. This number is a comparative value, not a limit for a specific application.
avoidance
- Material selection according to medium: for chloride contact, molybdenum-alloyed grades such as 1.4404
- Complete removal of Temper colors after welding Pickling and passivation, brushing with stainless steel brushes or grinding
- Root protection (Forming) during welding to prevent oxidation of the weld root
- Gapless design, no dead ends, complete emptying capability
- Separation of stainless steel and structural steel processing to prevent cross-contamination
- Smooth surfaces: lower roughness makes it harder for deposits to form.